Add to Cart
1.2344/ H13/ SKD61 Alloy Steel Plate and Flat Bar for Hot Work Tool Steel
Equivalent Grades
GB | DIN | AISI | JIS | ASSAB |
4Cr5MoSiV1 | 1.2344 | H13 | SKD61 | 8407 |
Features
a, Electro slag remelting, annealing with diffusion process and ultrafining heat-treatment has good microstructua homogeneity and finer dispersed carbides.
b, High isotropy, aspect rations≥0.8
c, Good tempering performance, high toughness, high temperature strength, good thermal stability and thermal fatigue resistance.
d, Annealing hardness≤230HB,quenching hardness 51-55HRC,tempering hardness 46-50HRC
Available Size (mm)
Flat Bar Size(mm) | Round bar Size(mm) | |||
Thickness | Width | Length | Diameter | Length |
16-260 | 205-610 | 3000-6000 | 16-200 | 300-6000 |
Chemical Composition (%)
Grade | C | Si | Mn | P | S | Cr | Mo | V |
H13 | 0.32-0.45 | 0.80-1.20 | 0.20-0.50 | ≤0.030 | ≤0.030 | 4.75-5.50 | 1.10-1.75 | 0.80-1.20 |
SKD61 | 0.32-0.42 | 0.80-1.20 | 0.20-0.50 | ≤0.030 | ≤0.030 | 4.75-5.50 | 1.10-1.75 | 0.80-1.20 |
1.2344 | 0.38-0.42 | 0.80-1.20 | 0.30-0.50 | ≤0.015 | ≤0.020 | 4.80-5.50 | 1.20-1.50 | 0.90-1.10 |
4Cr5MoSiV1 | 0.32-0.45 | 0.80-1.20 | 0.20-0.50 | ≤0.030 | ≤0.030 | 4.75-5.50 | 1.10-1.75 | 0.80-1.20 |
Recommend Heat Treatment
quenching | tempering | ||||||
Heating temperature/℃ | Cooling way | Hardness (HRC) | Tempering temperature /ºC | Tempering number | Hardness (HRC) | ||
First preheating | Second preheating | Last heating | |||||
500-550 | 750-800 | 1020-1050 | Oil Cooling or Air Cooling | 56-58 | 560-580 | 3 | 40-45 |